This product uses ceramic fiber as the main material and adds a certain proportion of airgel powder or particles to achieve a good heat insulation effect.
project
Model parameters
Testing standards
HD-XWN-01
HD-XWN-02
HD-XWN-03
in container
state
Pasty, no lumps, uniform
JG/T24-2000
thermal conductivity
0.038 W/(m·K)
0.032 W/(m·K)
0.028 W/(m·K)
GB/T14907-2018
density
60~100g/l
80~150g/l
90~150g/l
GB/T4472-2011
Construction and polishability
Can be polished by hand,
Smooth surface after grinding
GB/T1770-2008
Drying time
4~12h
GB/T1728-1979
water resistance
No exception ( 96h )
GB/T1733-1993
Alkali resistance
No exception ( 48h )
GB/T9265-2009
Bonding strength ( MPa )
≥0.7
GB/T9775-2015
Flexibility
Passed